ASTM A384/A384M-02 - 10.10.2002
 
1. Scope

1.1 Steel assemblies and subassemblies fabricated by welding, such as composite structural members, sash, weldments, etc., that are to be hot-dip galvanized after fabrication, are subject to warpage and distortion of the material due to the heating and cooling incidental to the galvanizing operation, particularly when it is necessary for the assembly to be dipped more than once to cover the entire surface.

1.2 This specification is applicable in either inch pounds or SI units. Inch pounds and SI units are not necessarily exact equivalents. Within the text of this specification and where appropriate, SI units are shown in parentheses.

 
2. Referenced Documents

A143/A143M-07(2020)

Standard Practice for Safeguarding Against Embrittlement of Hot-Dip Galvanized Structural Steel Products and Procedure for Detecting Embrittlement

A780-01

Standard Practice for Repair of Damaged and Uncoated Areas of Hot-Dip Galvanized Coatings

A385-08

Standard Practice for Providing High-Quality Zinc Coatings (Hot-Dip)