ASTM A439/A439M-18(2022) - 1.10.2022
 
1. Scope

1.1?This specification covers austenitic ductile iron castings, which are used primarily for their resistance to heat, corrosion, and wear, and for other special purposes.

1.2?Austenitic ductile iron, also known as austenitic nodular iron or austenitic spheroidal iron, is characterized by having its graphite substantially in a spheroidal form and substantially free of flake graphite. It contains some carbides and sufficient alloy content to produce an austenitic structure.

1.3?The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in nonconformance with the standard.

1.4?This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

 
2. Referenced Documents

A247-19

Standard Test Method for Evaluating the Microstructure of Graphite in Iron Castings

E351-18

Standard Test Methods for Chemical Analysis of Cast Iron“All Types

E59-93

Practice for Sampling Steel and Iron for Determination of Chemical Composition (Withdrawn 1996)

E30-89

Test Methods for Chemical Analysis of Steel, Cast Iron, Open-Hearth Iron, and Wrought Iron (Withdrawn 1995)

E10-23

Standard Test Method for Brinell Hardness of Metallic Materials

A370-23

Standard Test Methods and Definitions for Mechanical Testing of Steel Products

E8-04

Standard Test Methods for Tension Testing of Metallic Materials