ASTM C1113-99 - 10.3.1999
 
1. Scope

1.1 This test method covers the determination of the thermal conductivity of non-carbonaceous, dielectric refractories.

1.2 Applicable refractories include refractory brick, refractory castables, plastic refractories, ramming mixes, powdered materials, granular materials, and refractory fibers.

1.3 Thermal conductivity k-values can be determined from room temperature to 1500°C, or the maximum service temperature limit of the refractory, or to the temperature at which the refractory is no longer dielectric.

1.4 This test method is applicable to refractories with k-values less than 15 W/m[dot]K (100 Btu[dot]in./h[dot]ft2[dot]°F).

1.5 In general it is difficult to make accurate measurements on anistropic materials, particularly those containing fibers, and the use of this test method for such materials should be agreed between the parties concerned.

1.6 The values stated in SI units are to be regarded as standard.

1.7 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

 
2. Referenced Documents

E691-23

Standard Practice for Conducting an Interlaboratory Study to Determine the Precision of a Test Method

DIS*8894-2

Refractory Materials - Determination of Thermal Conductivity up to 1250C of Dense and Insulating Refractory Products According to the Hot Wire Parallel Method

C865-22

Standard Practice for Firing Refractory Concrete Specimens

C201-24

Standard Test Method for Thermal Conductivity of Refractories

C134-95(2023)

Standard Test Methods for Size, Dimensional Measurements, and Bulk Density of Refractory Brick and Insulating Firebrick